SPVC 71S is a free flowing vinyl chloride homopolymer resin having high molecular weight. It is manufactured by suspension polymerization. SPVC 71S has following properties that make it suitable for plasticized PVC processing:
High porosity (Excellent plasticizer absorption)
, Low content of fines (Easy handling and conveying)
, Good di-electrical properties (Good electrical insulation properties)
, Good transparency and low gels content (Good for transparent applications)Information provided by SABIC |