MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt SILVALOY® 071 (BRAZE™ 071, SILVALOY® B7T) Copper Silver Tin Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: Silvaloy 071 flows well on steels, without the use of flux, in controlled atmosphere furnace brazing. It can be used in place of copper brazing in many applications. Silvaloy 071 has also been used where a high temperature brazing alloy is required because it is desired to heat-treat steel after brazing. The small degree of melting that occurs in Silvaloy 071 at 1225°F does not appear to interfere with such applications. Silvaloy 071 is a low cost, high temperature silver brazing filler metal with an extremely long (580°F) melting range. Generally, it is not recommended for torch brazing but flows well on carbon steels, without flux, when used in a reducing furnace atmosphere.

Available forms: Wire, strip, engineered preforms, specialty preforms.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.89 g/cc8.89 g/cc
Density 8.89 g/cc0.321 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000135 ohm-cm0.0000135 ohm-cm12.8% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point 662.8 - 985.0 °C1225 - 1805 °F
Solidus 662.8 °C1225 °F
Liquidus 985.0 °C1805 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 985.0 - 1041 °C1805 - 1905 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 84 - 86 %84 - 86 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 6.5 - 7.5 %6.5 - 7.5 %
Tin, Sn 7.5 - 8.5 %7.5 - 8.5 %
 
Descriptive Properties
ColorYellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLUCM9837 / 254782

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.