MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nouryon Methyl Chloride methylchloride
Categories: Other Engineering Material

Material Notes: Methyl Chloride is used in the chemical and pharmaceutical industry, mainly as raw material for the production of silicones and methyl celluloses, but also for surfactants, pharmaceuticals and dye stuffs. For more information on Methyl Chloride, please download our Application Guide or Product Data Sheet.

CAS number: 74-87-3

REACH number: 01-2119493708-22

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.363 g/cc0.0131 lb/in³
 0.921 g/cc
@Pressure 1.013e-8 MPa,
Temperature 20.0 °C
0.0333 lb/in³
@Pressure 0.000001469 psi,
Temperature 68.0 °F
liquid
 1.003 g/cc
@Pressure 0.00001013 MPa,
Temperature -24.0 °C
0.03624 lb/in³
@Pressure 0.001469 psi,
Temperature -11.2 °F
liquid
 2.307 g/cc
@Pressure 0.00001013 MPa,
Temperature 0.000 °C
0.08335 lb/in³
@Pressure 0.001469 psi,
Temperature 32.0 °F
gas
Viscosity 0.18 cP0.18 cP
Molecular Weight 50.49 g/mol50.49 g/mol
Surface Tension 16.5 dynes/cm16.5 dynes/cm(liquid), 4.90 bar
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 12.9
@Temperature -24.0 °C
12.9
@Temperature -11.2 °F
liquid
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 127.4 J/g
@Temperature -97.7 °C
54.81 BTU/lb
@Temperature -144 °F
Flash Point -46.0 °C
@Pressure 0.00001013 MPa
-50.8 °F
@Pressure 0.001469 psi
in air
Ignition Temperature 625 °C
@Pressure 0.00001013 MPa
1160 °F
@Pressure 0.001469 psi
 
Descriptive Properties
Freezing point97.7 °C
Heat of combustion-12790 J/gΔHc° (gas), 25°C, 1013 mbar
 -1622 J/gΔHf° (liquid), 25°C, 1013 mbar

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY686 / 286209

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.