MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DowAksa CFB20T Mid Weight Bidirectional Carbon Fabric Laminate
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: DowAksa CFB20T is a medium weight, high tensile strength bidirectional carbon fabric. It easily wets out with CarbonBond™ 300 Saturant Resin System and can be installed using the “wet lay-up” technique. This fabric has excellent mechanical properties.

CFB20T Carbon Fabric is designed to fabricate on-site composite reinforcements to a variety of structures and substrates: Flexural and shear reinforcement of beams; In-plane and out-of-plane reinforcement of concrete and masonry walls; Column wrapping and reinforcement of slab; Structural steel applications

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption  0.29 %
@Time 86400 sec
0.29 %
@Time 24.0 hour
ASTM D570
 0.70 %
@Time 605000 sec
0.70 %
@Time 168 hour
ASTM D570
Thickness 813 microns32.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Tensile Strength 703 MPa102000 psiASTM D3039
Elongation at Break 2.0 %2.0 %ASTM D3039
Tensile Modulus 33.8 GPa4900 ksiASTM D3039
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 0.900 µm/m-°C0.500 µin/in-°FASTM E831
CTE, linear, Transverse to Flow 53.5 µm/m-°C29.7 µin/in-°FASTM E831
Maximum Service Temperature, Air 300 °C572 °FHDT load not reported; ISO 75-1
Glass Transition Temp, Tg 98.9 °C210 °FASTM E1640

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWAK979 / 287926

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.