MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Solaxis PC 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts that withstand functional testing. A PC part manufactured on a Fortus® 3D Printer is 5 to 60 percent stronger than a part made on previous FDM® systems. It also has superior mechanical properties to ABS and a number of other thermoplastics. When combined with a Fortus 3D Printer, PC gives strong parts for conceptual modeling, functional prototyping, manufacturing tools, and production parts. PC runs the Xtend 500 Fortus Plus option, which enables more than 400 hours of unattended build time.

Information provided by Solaxis Ingenious Manufacturing

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 115ASTM D785
Tensile Strength, Ultimate 42.0 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 57.0 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Strength, Yield 30.0 MPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 40.0 MPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Break 2.5 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 4.8 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Elongation at Yield 2.0 %
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
 2.2 %
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
Tensile Modulus 1.944 GPa
@Thickness 3.17 mm
XZ Axis, Type 1, 0.2 in./min; ASTM D638
 1.958 GPa
@Thickness 3.17 mm
ZX Axis, Type 1, 0.2 in./min; ASTM D638
Flexural Strength 68.0 MPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 89.0 MPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Modulus 1.80 GPaZX Axis, Method 1, 0.05 in./min; ASTM D790
 2.006 GPaXZ Axis, Method 1, 0.05 in./min; ASTM D790
Flexural Strain at Break >= 4.0 %ZX Axis, Method 1, 0.05 in./min; ASTM D790
Compressive Yield Strength 64.0 MPaZX Axis, Method 1, 0.05"/min; ASTM D695
 69.0 MPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Compressive Strength 65.0 MPaZX Axis, Method 1, 0.05"/min; ASTM D695
 193 MPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Compressive Modulus 1.56 GPaZX Axis, Method 1, 0.05"/min; ASTM D695
 7.56 GPaXZ Axis, Method 1, 0.05"/min; ASTM D695
Izod Impact, Notched 28.0 J/mZX Axis, Method A; ASTM D256
 73.0 J/mXZ Axis, Method A; ASTM D256
Izod Impact, Unnotched 187 J/mZX Axis, Method A; ASTM D256
 877 J/mXZ Axis, Method A; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+13 - 2.00e+14 ohm-cmASTM D257
Dielectric Constant 2.8 - 3.0ASTM D150-98
Dielectric Strength 80.0 - 360 V/milASTM D149-09, Method A
Dissipation Factor 0.0050 - 0.0060ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°CASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 138 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CASTM D648
Vicat Softening Point 139 °CASTM D1525
Glass Transition Temp, Tg 161 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLXIS987 / 256144

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.