MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® Endure D5G3 BM BK20560 (Dry) Nylon 66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Ultramid Endure D5G3 BM BK20560 is a glass fiber reinforced blow molding grade with good sagging behavior, ideal swelling and excellent heat aging resistance up to at least 220 degC (428 degF).

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  15.0 MPa
@Temperature 23.0 °C
2180 psi
@Temperature 73.4 °F
ISO 527
 46.0 MPa
@Temperature 150 °C
6670 psi
@Temperature 302 °F
ISO 527
Elongation at Break  5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
ISO 527
 17 %
@Temperature 150 °C
17 %
@Temperature 302 °F
ISO 527
Tensile Modulus  1.70 GPa
@Temperature 150 °C
247 ksi
@Temperature 302 °F
ISO 527
 5.50 GPa
@Temperature 23.0 °C
798 ksi
@Temperature 73.4 °F
ISO 527
Charpy Impact Unnotched  4.80 J/cm²
@Temperature -30.0 °C
22.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 8.40 J/cm²
@Temperature 23.0 °C
40.0 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  0.440 J/cm²
@Temperature -30.0 °C
2.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 34.0 µm/m-°C18.9 µin/in-°F
CTE, linear, Transverse to Flow 95.0 µm/m-°C52.8 µin/in-°F
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Blow-up Ratio (BUR) 2.02.0
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
176 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.050 %<= 0.050 %Optimal
 <= 0.12 %<= 0.12 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8977 / 254935

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.