MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Terves TervAlloy™ 1132 (FW+) Dissolvable Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: TervAlloy™ 1132 (FW+) is the latest freshwater version of Terves’ patented dissolvable magnesium designed for oil and gas applications. This alloy presents the best of both worlds – dissolution at extremely low salinity levels (1000 ppm) with mechanical characteristics comparable to our market-leading TervAlloy™ 3241 (TAx100E). TervAlloy 1132 is designed to provide our customers with the ideal product in applications where little salt content exists or where a very fast dissolving product is needed. TervAlloy 1132 provides mechanical performance previously unseen in any dissolvable alloy capable of responding to minimal salinity. TervAlloy 1132 can be purchased in the same broad range of shapes offered across the TervAlloy range (including cost-saving tubulars) in lengths up to 48 inches (in increments of 6 inches), and also in frac ball configurations up to 4.95 inches in diameter.

Information provided by Terves Incorporated

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 37.0 ksi4" Solid Rod, 5:1 Extrusion Ratio
Tensile Strength, Yield 25.0 ksi4" Solid Rod, 5:1 Extrusion Ratio
Elongation at Break 9.0 %4" Solid Rod, 5:1 Extrusion Ratio, Longitudinal values
Compressive Strength 52.6 ksi4" Solid Rod, 5:1 Extrusion Ratio
Shear Strength 19.1 ksi4" Solid Rod, 5:1 Extrusion Ratio, Double Shear
 
Descriptive Properties
Dissolution Data11 mg/cm2hr0.1% KCl, 60°C
 117 mg/cm2hr3% KCl, 90°C
 13 mg/cm2hr1.0% KCl, 30°C
 16 mg/cm2hr3% KCl, 30°C
 21.5 mg/cm2hr0.1% KCl, 90°C
 4 mg/cm2hr0.1% KCl, 30°C
 48 mg/cm2hr1.0% KCl, 60°C
 56 mg/cm2hr3% KCl, 60°C
 75 mg/cm2hr1.0% KCl, 90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTERVES010 / 314477

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.