MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical KSS Non-Halogenated Flame Retardant for PC
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: Potassium diphenyl sulfone sulfonate

CAS No. 63316-43-8

GOYENCHEM-KSS is a sulfonate highly effective nonhalogenated flame retardant which is particularly for polycarbonate (PC). It provides excellent flame retardancy and thermal stability. The transparency of PC engineering products will not be affected by the additive and therefore GOYENCHEM-KSS can be applied to various transparent and colored products.

Intro: GO YEN CHEMICAL CO. LTD. currently is the largest functional specialty chemical manufacturer in Taiwan which is continuously pursuing and developing products that take environmental protection and marketing requirements into account, then help customers to research and develop new products after understanding their requirements in order to solve customers’ problems and meet their demands. GOYENCHEM-KSS is a sulfonate highly effective nonhalogenated flame retardant which is particularly for polycarbonate (PC). It provides excellent flame retardancy and thermal stability. The transparency of PC engineering products will not be affected by the additive and therefore GOYENCHEM-KSS can be applied to various transparent and colored products.

Features/Benefits:

  • Remarkable flame retardant effect
  • Provides great flame retardant effect with a minimal amount
  • High heat resistance
  • Eco-friendly non-halogenated flame retardant
  • Non-blooming and shows great anti-migration properties after adding into PC
  • Barely affects the mechanical properties of PC
  • Can be used in any transparent or colored PC products, or either in PC/ABS to improve its physical properties and flame retardancy
  • Can be used individually or with GYC phosphate flame retardant
Applications:
  • Various transparent or colored PC products
  • PC granulation
  • PC injection
  • PC/ABS

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.5 - 7.56.5 - 7.5
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.8 %<= 1.8 %
 
Descriptive Properties
AppearancePowder
ColorWhite
Composition<0.5%DPs Content
 <5 ppmIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN001 / 266309

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.