Product Description: TRIREX is the registered trademark of polycarbonate resin manufactured by Samyang Corporation. TRIREX polycarbonate resins offer superior mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries. TRIREX 3027U(H) is a polycarbonate resin grade which has low temperature impact strength in combination with superior mechanical and physical property. Characteristics: Superior low temperature impact resistance; Good flow-ability; Workable under a wide range of temperatures (-100-135°C); High electrical performance; Good dimensional stability; Low moisture absorbency; Good weather resistance Applications: TRIREX 3027U(H) resin grade is designed for Injection molding components. UV stabilized. Medium high viscosity. Transparent colors only. Availability: Asia Pacific; Europe; North America Additive: UV Stabilizer Features: Good Dimensional Stability; Good Electrical Properties; Good Flow; Good Weather Resistance; Low Moisture Absorption; Low Temperature Impact Resistance; Medium Viscosity Uses: Appliances; Automotive Applications; Electrical/Electronic Applications; Optical Applications Appearance: Clear/Transparent Form: Pellets Processing Method: Injection Molding Information provided by Samyang Corporation |