MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Angst+Pfister APSOplast® PEEK SL PEEK + carbon fibre + graphite + PTFE
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled; Polyetheretherketone, PEEK, PTFE-Filled

Material Notes: The addition of carbon fibre, PTFE, and graphite gives this PEEK slide bearing material exceptional tribological properties (low coefficient of friction, high wear resistance, and high PV limit value) and makes it into the ideal material for components subject to high wear, friction, and thermal and mechanical loads.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³DIN EN ISO 1183-1
Water Absorption  0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
DIN EN ISO 62
 0.030 %
@Time 346000 sec
0.030 %
@Time 96.0 hour
DIN EN ISO 62
Moisture Absorption 0.150 %0.150 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585DIN EN ISO 868
Ball Indentation Hardness 220 MPa31900 psiDIN EN ISO 2039-1
Tensile Strength, Yield 75.0 MPa10900 psiDIN EN ISO 527
Elongation at Break 4.0 %4.0 %DIN EN ISO 527
Modulus of Elasticity 4.90 GPa711 ksiDIN EN ISO 527
Charpy Impact Unnotched 2.80 J/cm²13.3 ft-lb/in²DIN EN ISO 179-1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+7 - 1.00e+9 ohm-cm1.00e+7 - 1.00e+9 ohm-cmIEC 60093
Surface Resistance 1.00e+7 - 1.00e+9 ohm1.00e+7 - 1.00e+9 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear  30.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 140 °F
 30.0 µm/m-°C
@Temperature 23.0 - 150 °C
16.7 µin/in-°F
@Temperature 73.4 - 302 °F
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Melting Point 343 °C649 °FISO 11357-3
Maximum Service Temperature, Air 250 °C482 °Flong term
 310 °C590 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 150 °C302 °FDIN EN ISO 75 / A
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP060 / 250558

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.