MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical GOYENCHEM-359 High-Performance Anti-Sticking Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEM-359 was developed by GO YEN CHEMICALINDUSTRIAL CO., LTD. (GYC Group) technologydepartment for customers who specialize in synthetic sheet,resin and coating film. It can replaces Japanese andGerman manufactures to improve the flowability and smoothness of coating film and improve the touch. Enhance the added value of products and it is the designate products for well-known international paint manufacturers.

Advantages:

  • Provide outstanding flowability and smoothness to the coating
  • Excellent weather resistance
  • Provides a smooth texture of resin, ink and paint
  • Great compatibility with various coating and resins
  • Prevent surface defects, shrinkage holes and other defects
  • Give anti-adhesion property
Applications:
  • All kinds of oleic resins
  • Polyurethane resin
  • Acrylic resin
  • Epoxy resin
  • Vacuum plating aluminum film
  • Synthetic plate
  • Amino acid
  • DAP, Polyester
  • Cellulose

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/inĀ³
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.401.40
 
Descriptive Properties
AppearanceLiquid
ColorTransparent colorless
Composition1Valid content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN411 / 266719

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.