MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

JSC Agidol feed grade, sort P
Categories: Other Engineering Material

Material Notes: Ingredients: Butylated hydroxytoluene (BHT) E321, CAS # 128-37-0
Anticaking agent Silicon dioxide E551b, CAS # 7631-86-9Agidol feed grade, sort P is a mixture of butylated hydroxytoluene (BHT) and anticaking agent Silicon dioxide. The product is designed to stabilize fat-soluble vitamins (A, D, E), fats and other labile components in complete feeds and premixes, fish and meat and bone meal, carotene in herbal meal, as well as to increase the productivity of farm animals, including birds.

REACH: Complies with requirements of Regulation (EC) No. 1831/2003 on additives for use in animal nutrition.

CAS: Butylated hydroxytoluene (BHT) E321, CAS # 128-37-0

CAS: Anticaking agent Silicon dioxide ?551b, CAS # 7631-86-9

Empirinc Formula of BHT: C15H24O

Empiric formula of silicon dioxide: SiO2

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash 1.5 - 2.0 %1.5 - 2.0 %
Storage Temperature -30.0 - 40.0 °C-22.0 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Crystallization Temperature <= 68.2 °C<= 155 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Appearancewhite crystalline powder without foreign impurities
Content< 0.5 ng WHO-PCDD/F-TEQ/kgDioxins
 <0.3%Other alkyl phenols (except Agidol-1 and phenol) content, in the sum of tert-butylphenols
 <1.5 ng WHO-PCDD/F-TEQ/kgSum of dioxins and dioxin-like PCBs
 <10 mg/kgNon-dioxin-like PCBs
 <2 mg/kgCadmium
 <30 mg/kgLead
 0.5 ng WHO-PCDD/F TEQ/kgDioxin-like PCBs
 97.7-98.5%4-methyl-2,6-di-tert-butylphenol (Agidol-1)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSC006 / 317826

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.