MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL GTX™ Resin GTX918A Polyphenylene Ether + PA (PPE+Nylon)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 918A resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, high melt flow, and added mold release. NORYL GTX918A resin may be an excellent candidate for automotive under-the-hood and electrical applications requiring the retention of properties while under thermal load.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Water Absorption at Saturation 4.2 %4.2 %ASTM D570
Viscosity 5.0 cP
@Load 1.20 kg,
Temperature 280 °C
5.0 cP
@Load 2.65 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm
@Thickness 3.20 mm
0.013 - 0.016 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.013 cm/cm
@Thickness 3.20 mm
0.010 - 0.013 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 280 °C
45 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psi50 mm/min; ISO 527
 57.0 MPa8270 psi50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa8700 psi50 mm/min; ISO 527
 62.0 MPa8990 psi50 mm/min; ASTM D638
Elongation at Break 30 %30 %50 mm/min; ISO 527
 53 %53 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %4.5 %50 mm/min; ISO 527
 11.4 %11.4 %50 mm/min; ASTM D638
Flexural Strength 85.0 MPa12300 psiyield, 2 mm/min; ISO 178
 98.0 MPa14200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.20 GPa319 ksi2 mm/min; ISO 178
 2.36 GPa342 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 202 J149 ft-lbASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 40.0 J29.5 ft-lbpeak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
36.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow  68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 188 °C
@Thickness 3.20 mm
370 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
@Thickness 3.20 mm
298 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 190 °C374 °FRate B/50; ISO 306
 195 °C383 °FRate B/120; ISO 306
 242 °C468 °FRate B/50; ASTM D1525
 245 °C473 °FRate A/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 295 °C518 - 563 °F
Zone 2 260 - 295 °C500 - 563 °F
Zone 3 265 - 295 °C509 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82165 / 290112

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.