The diverse properties of virgin, unfilled PTFE are particularly in demand for anti-adhesive coatings, sliding functions with extremely low friction values, dielectric materials for high- voltage and HF applications, and for applications where the material comes into direct contact with aggressive chemicals and foodstuffs.Information provided by Angst + Pfister |