This PPE is reinforced with 30% glass fibre. In comparison with versions which are not reinforced, it has even better mechanical and thermal properties and higher dimensional stability. Moreover, it retains excellent electrical properties and resistance to hydrolysis.Information provided by Angst + Pfister |