MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Shanghai Potomer UV-326 Ultraviolet Absorbent Light Stabilizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS NO. 3896-11-5

Characteristics and Uses: UV-326 is a light stabilizer, capable of absorbing the ultraviolet radiation of 270-380 nanometers, mainly applied to polyvinylchloride, polystyrene, unsaturated resin, polycarbonate, poly (methyl methacrylate), polyethylene, ABS resin, epoxy resin and cellulose resin. This product almost does not absorbing visible light, particular applicable able to colorless transparent products and colored products. Dosage:0.1-0.5% for thin products and 0.05-0.2% for thick products. It can be applied to plastic products for packing foods.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 137 - 141 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 97 %
@Wavelength 460 nm
 >= 98 %
@Wavelength 500 nm
 
Descriptive Properties
Color/AppearanceLight Yellow Crystalline Powder
Loss on Drying<0.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM106 / 284552

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.