MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot VULCAN® 7H-C Reinforcing Carbon
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: VULCAN® 7H-C circular reinforcing carbon, powered by EVOLVE™ Sustainable Solutions, is a reinforcing material made from ISCC PLUS certified tire pyrolysis oil (TPO). Products produced using TPO offer the same quality and performance as Cabot’s traditional reinforcing carbons and can be used as drop-in solutions. ISCC is a globally leading certification system for feedstocks and markets to ensure sustainable content and traceability in supply chains.

Performance Features: VULCAN 7H-C circular reinforcing carbon conforms to ASTM N234 carbon black target values and is higher in surface area and structure than other tire tread products such as ASTM N220 and ASTM N339 type carbon blacks. It disperses well and gives moderately high modulus while imparting excellent extrusion characteristics to rubber compounds. Compared to ASTM N300 series and ASTM N220 type carbon blacks, VULCAN 7H-C circular reinforcing carbon enhances wear resistance in tire tread compounds. VULCAN 7H-C circular reinforcing carbon can offer up to 10% better tread wear resistance than a standard ASTM N220 type carbon black. VULCAN 7H-C circular reinforcing carbon provides, via ISCC PLUS mass balance approach, the possibility to increase the sustainable content in the final application with drop-in performance versus standard VULCAN 7H-C carbon black.

Typical Applications: VULCAN 7H-C circular reinforcing carbon is particularly well suited for synthetic and natural rubber-based tire treads that require excellent wear resistance. It is also recommended for conveyor belts, solid tires, and other industrial rubber products requiring excellent abrasion resistance, such as: Treads of premium passenger car tires, truck tires and solid tires; Truck tire retreads; Conveyor belts

Technical Data: Test Formulation: 89 phr SBR1712, 35 ph BR, 11 phr Free oil

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 52
@Temperature 100 °C
52
@Temperature 212 °F
ML (1+4)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858
Tensile Strength 21.0 MPa3050 psi
Elongation at Break 585 %585 %
300% Modulus 7.50 MPa1090 psi
Resilience 100100Cured 70’% relative to VULCAN® 7H-C; ASTM D1054
 100100Tread Wear Rating Index; ASTM D1054
 
Thermal PropertiesMetricEnglishComments
Shrinkage 100 %100 %Extrusion, Method B, % Relative to VULCAN® 7H-C; ASTM D2230

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT012 / 315747

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.