MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Intene® 30 AF High CIS Polybutadiene Polymer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Intene® 30 AF is a solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst at the Grangemouth production facility in Scotland, UK. A TNPP free, food contact approved, non-staining antioxidant is added during the production process.

Applications: Impact improver of ABS and Polystyrene giving a gloss surface. It can also be used in conjunction with certain block copolymers to give high gloss. The high capacity of loading carbon black and good extrudibility makes this grade suitable for abrasion strips construction in tire building.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.75 %ASTM D 5668
Viscosity 65 cP
@Temperature 25.0 °C
5 wt% in styrene solution; Internal Method
Ash <= 0.10 %ASTM D 5667
 
Descriptive Properties
Cis- 1:4 Content (%)38Internal Method
Color5Internal Method. 5% wt./wt. in Styrene at 25°C.
Gel Rating5 maxInternal Method. 5% wt./wt. in Styrene at 25°C.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9927 / 265640

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.