MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer ML6411 Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.0mm flame retardancy based on non-chlorine, non-bromine FR systems. LEXAN ML6411 resin offers excellent processing characteristics with opportunity for shorter IM cycle times compared to standard PC. This product is available in a wide range of opaque colors and is an excellent candidate for a wide range of electrical applications.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ISO 62-1
Viscosity 18 cP
@Load 5.00 kg,
Temperature 260 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 54.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
 62.0 MPa50 mm/min; ISO 527
Elongation at Break 100 %50 mm/min; ASTM D638
 100 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ASTM D638
 5.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1 mm/min; ISO 527
 2500 MPa50 mm/min; ASTM D638
Flexural Strength 90.0 MPayield, 2 mm/min; ISO 178
 95.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2350 MPa2 mm/min; ISO 178
 2600 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 900 JASTM D256
 150 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 60.0 kJ/m²80*10*3; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Dart Drop, Total Energy 72.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Dielectric Strength 26.5 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Comparative Tracking Index 250 VIEC 60112
 250 - 400 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.750 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.750 mm
UL 746A
 >= 120 arcs
@Thickness >=1.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 59.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 125 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 128 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 114 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 119 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 134 °CRate B/50; ASTM D1525
 134 °CRate B/50; ISO 306
 135 °CRate B/120; ISO 306
UL RTI, Electrical 100 °CUL 746B
UL RTI, Mechanical with Impact 100 °CUL 746B
UL RTI, Mechanical without Impact 100 °CUL 746B
Flammability, UL94 V-2
@Thickness >=0.750 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 5VB
@Thickness >=1.70 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
Glow Wire Ignition Temperature 800 °C
@Thickness 0.750 mm
IEC 60695-2-13
 800 °C
@Thickness 1.00 mm
IEC 60695-2-13
 800 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 1.70 mm
IEC 60695-2-13
 800 °C
@Thickness 2.00 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 1.70 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 290 °C
Zone 2 250 - 290 °C
Zone 3 260 - 300 °C
Melt Temperature 270 - 300 °CInjection Molding
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80405 / 288352

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.