MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ STAT-KON™ Compound DX13315C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX13315C compound is based on Polycarbonate (PC) resin containing 15% carbon fiber. Added features of this grade include: LNP Clean Compounding Technology, Low LPC, Low Ionics, Low Outgassing, Low C18-C40 Hydrocarbons, Electrically Conductive.

Features: LNP Clean Compound Technology,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.26 g/cc1.26 g/ccASTM D792
Viscosity 30 cP
@Load 5.00 kg,
Temperature 300 °C
30 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0050 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 129 MPa18700 psi5 mm/min; ASTM D638
 130 MPa18900 psi5 mm/min; ISO 527
Elongation at Break 2.6 %2.6 %5 mm/min; ISO 527
 2.7 %2.7 %5 mm/min; ASTM D638
Tensile Modulus 10.41 GPa1510 ksi5 mm/min; ASTM D638
 10.64 GPa1543 ksi1 mm/min; ISO 527
Flexural Strength 199 MPa28900 psiASTM D790
 203 MPa29400 psiyield, 2 mm/min; ISO 178
Flexural Modulus 9.17 GPa1330 ksiASTM D790
 9.29 GPa1350 ksi2 mm/min; ISO 178
Izod Impact Notched 88.0 J64.9 ft-lbASTM D256
Izod Impact, Unnotched 5.91 J/cm11.1 ft-lb/inASTM D4812
Charpy Impact Unnotched 4.50 J/cm²21.4 ft-lb/in²ISO 179/2C
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/2C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 50000 - 5.00e+6 ohm-cm50000 - 5.00e+6 ohm-cmASTM D257
Surface Resistance 5000 - 500000 ohm5000 - 500000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
7.78 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 123 °C
@Thickness 3.20 mm
253 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.00 mm
HB
@Thickness 0.0394 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 320 °C536 - 608 °F
Zone 2 280 - 320 °C536 - 608 °F
Zone 3 280 - 320 °C536 - 608 °F
Melt Temperature 280 - 320 °C536 - 608 °FInjection Molding
Mold Temperature 90.0 - 120 °C194 - 248 °F
Drying Temperature 90.0 - 110 °C194 - 230 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 1.00 - 5.00 MPa145 - 725 psi
Screw Speed 30 - 100 rpm30 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81267 / 289214

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.