System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ THERMOCOMP™ Compound LF003 Polyetheretherketone (PEEK)
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
Material Notes:
LNP THERMOCOMP LF003 compound is based on Polyetheretherketone (PEEK) resin containing 15% glass fiber.
Features: High Stiffness,High Heat Resistance,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.39
g/cc
ASTM D792
1.39
g/cc
ISO 1183
Linear Mold Shrinkage, Flow
0.0079
cm/cm
24hrs; ISO 294
0.0080
cm/cm
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.010
cm/cm
24hrs; ASTM D955
0.010
cm/cm
24hrs; ISO 294
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
125
MPa
ISO 527
136
MPa
ASTM D638
Tensile Strength, Yield
125
MPa
ISO 527
136
MPa
ASTM D638
Elongation at Break
2.3 %
ISO 527
3.1 %
ASTM D638
Elongation at Yield
2.3 %
ISO 527
2.9 %
ASTM D638
Tensile Modulus
6930
MPa
1 mm/min; ISO 527
7446
MPa
5 mm/min; ASTM D638
Flexural Strength
199
MPa
ASTM D790
209
MPa
ISO 178
Flexural Modulus
6274
MPa
ASTM D790
7000
MPa
ISO 178
Izod Impact Notched
53.0
J
ASTM D256
Izod Impact, Unnotched
854
J/m
ASTM D4812
Izod Impact, Notched (ISO)
6.00
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
54.0
kJ/m²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
14.0
J
peak; ASTM D3763
Impact Test
3.00
J
Multiaxial Impact; ISO 6603
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
30.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
31.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
48.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
48.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi)
325
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
328
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
244
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
258
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Processing Properties
Original Value
Comments
Zone 2
380
-
400
°C
Zone 3
380
-
400
°C
Mold Temperature
175
-
190
°C
Drying Temperature
150
°C
Injection Molding
Dry Time
4.00
-
6.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
Screw Speed
60
-
100
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH81684 / 289631
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.