MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL™ Resin SE1GFN2 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ SE1GFN2 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2mm and V1 at 1.5mm along with UL746C Outdoor Suitability rating of F1 and RTI of 110C. NORYL SE1GFN2 exhibits high heat resistance, good dielectric strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for a variety of applications such as solar frames, unattended power supply (UPS) inverter/charger, indoor and outdoor electrical enclosures / housings / connectors, and wall plates / sockets / switches.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Water Absorption 0.11 %
@Time 86400 sec
0.11 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Moisture Absorption at Equilibrium 0.040 %0.040 %23°C/50% RH; ISO 62-4
Viscosity 3.0 cP
@Load 5.00 kg,
Temperature 280 °C
3.0 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0050 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 280 °C
3.5 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 100 MPa14500 psi50 mm/min; ISO 527
 120 MPa17400 psi50 mm/min; ASTM D638
Elongation at Break 2.5 %2.5 %50 mm/min; ISO 527
 3.0 %3.0 %50 mm/min; ASTM D638
Tensile Modulus 6.40 GPa928 ksi1 mm/min; ISO 527
 7.10 GPa1030 ksi5 mm/min; ASTM D638
Flexural Strength 140 MPa20300 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 150 MPa21800 psiyield, 2 mm/min; ISO 178
Flexural Modulus 5.50 GPa798 ksi1.3 mm/min, 50 mm span; ASTM D790
 5.60 GPa812 ksi2 mm/min; ISO 178
Izod Impact Notched 100 J73.8 ft-lbASTM D256
 90.0 J
@Temperature -30.0 °C
66.4 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.20 J/cm9.74 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 28.0 kJ/m²13.3 ft-lb/in²80*10*4; ISO 180/1U
 27.0 kJ/m²
@Temperature -30.0 °C
12.8 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179/2C
Dart Drop, Total Energy 18.0 J13.3 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.04e+16 ohm-cm2.04e+16 ohm-cmASTM D257
 2.04e+16 ohm-cm2.04e+16 ohm-cmIEC 60093
Surface Resistance 1.34e+17 ohm1.34e+17 ohmASTM D257
 1.34e+17 ohm1.34e+17 ohmROA; IEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 2.93
@Frequency 1e+6 Hz
2.93
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength  26.2 kV/mm
@Thickness 1.50 mm
665 kV/in
@Thickness 0.0591 in
in oil; IEC 60243-1
 26.2 kV/mm
@Thickness 1.60 mm
665 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor  0.0034
@Frequency 1e+6 Hz
0.0034
@Frequency 1e+6 Hz
ASTM D150
 0.0034
@Frequency 1e+6 Hz
0.0034
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 - 400 V250 - 400 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=0.400 mm
30 - 60 sec
@Thickness >=0.0157 in
UL 746A
 >= 120 sec
@Thickness >=0.710 mm
>= 120 sec
@Thickness >=0.0280 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=0.400 mm
0.00 - 15 arcs
@Thickness >=0.0157 in
UL 746A
 30 - 60 arcs
@Thickness >=1.50 mm
30 - 60 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min>= 5.91 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  25.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 30.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
@Thickness 3.20 mm
288 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 133 °C271 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 134 °C
@Thickness 3.20 mm
273 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 142 °C288 °FRate B/50; ASTM D1525
 142 °C288 °FRate B/50; ISO 306
 144 °C291 °FRate B/120; ISO 306
UL RTI, Electrical 110 °C230 °FUL 746B
UL RTI, Mechanical with Impact 105 °C221 °FUL 746B
UL RTI, Mechanical without Impact 110 °C230 °FUL 746B
Flammability, UL94  V-1
@Thickness >=0.400 mm
V-1
@Thickness >=0.0157 in
UL 94
 5VA
@Thickness >=2.50 mm
5VA
@Thickness >=0.0984 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82469 / 290416

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.