LNP LUBRICOMP RFL36L compound is based on Nylon 6/6 resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Low Extractable. Features: Low Extractable,Wear resistant,Food Contact Acceptable,Structural Information provided by SABIC |