OKULEN® 1000 – UV black – FN9100 is a ultra high molecular low pressure polyethylene with a molecular weight of approx. 5.000.000 g/mol (UHMW-PE) Properties: UV stabilized; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: black FN9100/similar RAL9005 Range of applications: Mechanical engineering; Conveying industry; Outdoor applications Information provided by Okulen |