MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin N300X Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ N300X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2mm and V0 at 1.5mm. NORYL N300X resin offers strong electrical performance, low moisture absorption, dimensional stability, and hydrolytical stability. This material is an excellent candidate for indoor and outdoor electrical enclosure and solar / photovoltaic junction box applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Water Absorption at Saturation 0.060 %ASTM D570
Viscosity 7.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 7.4 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 119ASTM D785
Tensile Strength at Break 66.0 MPaISO 527
 73.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 74.0 MPa50 mm/min; ASTM D638
 75.0 MPaISO 527
Elongation at Break 7.6 %50 mm/min; ASTM D638
 13 %ISO 527
Elongation at Yield 5.2 %ISO 527
 5.3 %50 mm/min; ASTM D638
Tensile Modulus 2220 MPa1 mm/min; ISO 527
 2380 MPa5 mm/min; ASTM D638
Flexural Strength 110 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 110 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 112 MPaISO 178
Flexural Modulus 2500 MPa2.6 mm/min, 100 mm span; ASTM D790
 2520 MPaISO 178
 2650 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 190 JASTM D256
 55.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
Dart Drop, Total Energy 54.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Surface Resistance 1.00e+17 ohmASTM D257
Dielectric Constant 2.63
@Frequency 1e+6 Hz
ASTM D150
 2.68
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 19.4 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0031
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 >= 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 156 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 155 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 140 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 145 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 162 °CRate B/50; ISO 306
 164 °CRate B/120; ISO 306
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 V-0
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=2.00 mm
UL 94
Glow Wire Ignition Temperature 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 300 - 325 °C
Zone 2 275 - 320 °C
Zone 3 290 - 325 °C
Melt Temperature 300 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82368 / 290315

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.