MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar Carrier

Appearance: Clear silicone gum on polymer film

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.00 milFluorinated Ethylene Propylene Interleave
 1.50 milMylar Carrier
 23.0 - 27.0 milOverall
 23.0 - 27.0 milSide 1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65 - 75Compound Property
Tensile Strength >= 1150 psiCompound Property
Elongation at Break >= 300 %Compound Property
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 204 °C
Recommended Postcure Cycle
 15.0 min
@Temperature 177 °C
Recommended Cure Cycle
Shelf Life 3.00 Month
@Temperature 4.44 °C
From date of manufacture
 
Descriptive Properties
ColorNaturally Translucent
Total Product Weight (oz/yd2)21.8 - 25.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon 15370P020 0.020" (0.508 mm) Uncured Silicone Rubber on a Mylar Carrier
Rogers Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave
Rogers Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Rogers Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

PARL114 / 125300

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.