MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mateck Neodymium Gallate Substrate, NdGaO3
Categories: Ceramic; Oxide

Material Notes: Substrate single crystals for superconductivity

Key Words: NdGaO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.57 g/cc0.273 lb/in³
a Lattice Constant 5.426 Å5.426 Å
b Lattice Constant 5.496 Å5.496 Å
c Lattice Constant 7.707 Å7.707 Å
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2525
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.0 µm/m-°C6.11 µin/in-°F
Melting Point 1600 °C2910 °F
 
Descriptive Properties
Growth TechniquesCzochralski
Orientation(110)
Orientation Accuracy ( ° ), Max0.5
Parallelness ( ° ), max0.02
Polishingstandard: one side
Production MethodCzochralski grown
Roughness of surface (angstroms), max30
Scratchesnone
Standard Size (mm)10 x 10 x 1 or 0.5
Statemonocrystalline
Structureorthorhombic
Surface Qualitywith light microscope without defects
Tolerance of Length (mm)± 0.1
Tolerance of Thickness (mm)± 0.05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMAT006 / 87690

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.