MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of less than 1x10-4 ohm-cm. AA-DUCT 902LP is also characterized by a wide operating temperature range from –50 to +170°C. AA-DUCT 902LP is recommended for electronic bonding and sealing applications that require both fine electrical and mechanical properties.

Appearance: Silver

Cure Type: Heat cure or Room Temperature

Benefits:

  • High strength
  • Perfect bond
  • Cold solder for heat sensitive components
Mix Ratio by weight: 100:6/Resin:Hardener

Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.

Typical Application: Electrical, conductive, rmi/efi shielding, circuitry, printed circuit board and electronics repair

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.79 g/ccuncured
Solids Content 100 %reactive, uncured
Linear Mold Shrinkage 0.0030 in/incured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85cured
Tensile Strength 9500 psicured
Compressive Strength 14000 psicured
Shear Strength 9400 psiLap, cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.00010 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
Thermal Conductivity 100 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 min
@Temperature 120 °C
 5.00 min
@Temperature 100 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 180 minuncured
Shelf Life 12.0 Monthuncured
 
Descriptive Properties
ViscosityPasteuncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 7075-T6; 7075-T651
Aluminum 2024-T4; 2024-T351 (Included Extended Size/Shape Data)
Aluminum 2024-T4; 2024-T351
Alcoa 2324-T39 Aluminum Plate
Alclad Aluminum 7075-T6, T651

PATOM034 / 172349

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.