MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX840 Polyphenylene Ether + PA (PPE+Nylon) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 840 resin is a 40% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade has high stiffness (flexural modulus 11860 MPa), excellent chemical resistance, and high heat resistance. NORYL GTX GTX840 resin is an excellent candidate for a wide variety of applications including automotive under-the-hood and water management.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Density 1.45 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ASTM D570
Viscosity 10 cP
@Load 5.00 kg,
Temperature 220 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0024 - 0.0027 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0063 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength at Break 178 MPa5 mm/min; ASTM D638
 198 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Tensile Modulus 13520 MPa5 mm/min; ASTM D638
 13940 MPa1 mm/min; ISO 527
Flexural Strength 249 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 280 MPayield, 2 mm/min; ISO 178
Flexural Modulus 11860 MPa1.3 mm/min, 50 mm span; ASTM D790
 12270 MPa2 mm/min; ISO 178
Izod Impact Notched 94.0 JASTM D256
 90.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 - 19.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 90.0 - 93.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 258 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 260 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 247 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 246 °CRate B/120; ISO 306
 246 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 295 - 315 °C
Zone 2 280 - 315 °C
Zone 3 290 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82152 / 290099

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.