MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Greene Tweed Arlon® 1330 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.

Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
Deformation 0.14 %0.14 %ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9696ASTM D785
Hardness, Shore D 8585ASTM D2240
Tensile Strength at Break 86.9 MPa12600 psiASTM D368
Tensile Strength, Yield 89.6 MPa13000 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Strength 145 MPa21100 psiASTM D790
Flexural Modulus 0.2031 GPa
@Temperature 204 °C
29.46 ksi
@Temperature 400 °F
 3.69 GPa
@Strain 0.5 %
535 ksi
@Strain 0.5 %
Secant; ASTM D790
Compressive Strength 107 MPa15500 psiASTM D695
Shear Strength 71.7 MPa10400 psiAxial; ASTM D732
 71.7 MPa10400 psiTransverse; ASTM D732
 14.3 MPa
@Temperature 288 °C
2080 psi
@Temperature 550 °F
 48.7 MPa
@Temperature 149 °C
7070 psi
@Temperature 300 °F
 68.3 MPa
@Temperature 65.6 °C
9900 psi
@Temperature 150 °F
Secant Modulus 3.59 GPa521 ksiTensile 0.5% Secant Modulus; ASTM D638
Coefficient of Friction, Dynamic 0.150.15PV=12600 psi-ft./min.; ASTM G77
K (wear) Factor 40.3 x 10-8 mm³/N-M20.0 x 10-10 in³-min/ft-lb-hrASTM G77
 
Thermal PropertiesMetricEnglishComments
CTE, linear  41.4 µm/m-°C
@Temperature <=149 °C
23.0 µin/in-°F
@Temperature <=300 °F
ASTM E228
 148 µm/m-°C
@Temperature >=149 °C
82.0 µin/in-°F
@Temperature >=300 °F
ASTM E228
Deflection Temperature at 1.8 MPa (264 psi) 166 °C330 °F
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Dry
Evonik VESTAKEEP® 1000P PEEK
Gharda Chemicals GATONE™ 5300 PEEK, High Viscosity Grade
Greene Tweed Arlon® 1000 Polyketone

PGREEN55 / 42349

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.