MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP5LTE-100 One component epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Unlimited working life at room temperature
  • Electrically insulating
  • Good flow properties
  • Moderate curing temperature
Product Description: Master Bond EP5LTE-100 is a flowable, one part epoxy with a low coefficient of thermal expansion. The curing schedule is 100°C for 90-120 minutes. Optimum properties are obtained by post curing for 2-3 hours at 100-125°C. The working life is unlimited because the epoxy will not cure until it reaches the elevated temperature. It should be emphasized that this system is not premixed and frozen and simply requires refrigeration for storage. EP5LTE-100 has very low shrinkage upon curing along with high dimensional stability. EP5LTE-100 bonds well to a wide variety of substrates including metals, glass, composites, ceramics and many plastics. It has a very good glass transition temperature of 120-125°C allowing it to be used in high temperature environments. The service temperature range is -60°C to +175°C. The coefficient of thermal expansion at 25°C is a remarkably low 8-12 x 10-6 in/in/°C. EP5LTE-100 has good resistance to water, oils, acids, bases and solvents. The color is brown. It can be used in electronic, aerospace, optical and specialty OEM type applications, among others, where a non-conductive, low CTE product is desirable. Some recent applications are in fiber optic packaging, including mounting optics and other components, and bonding fibers into ferrules. In microelectronics, low CTE’s are used for bonding SMDs and chips as well as die attaches and underfills. The main idea is that a low CTE epoxy will induce minimal stress upon bonded parts, especially during thermal cycling. This along with the high Tg of EP5LTE-100 is unusual and highly advantageous.

Product Advantages:

  • Not premixed and frozen
  • Easy to apply
  • Simple and straightforward cure schedule
  • High modulus
  • Well positioned glass transition temperature

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/cc
Viscosity 20000 - 160000 cP20000 - 160000 cPthixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85 - 9585 - 95
Tensile Strength 13.8 - 20.7 MPa2000 - 3000 psi
Elongation at Break <= 1.0 %<= 1.0 %
Tensile Modulus >= 6.89 GPa>= 1000 ksi
Compressive Strength 172 - 186 MPa25000 - 27000 psi
Adhesive Bond Strength 6.89 - 8.27 MPa1000 - 1200 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 12.0 µm/m-°C4.44 - 6.67 µin/in-°F
Thermal Conductivity 0.576 - 0.865 W/m-K4.00 - 6.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
Glass Transition Temp, Tg 120 - 125 °C248 - 257 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 120 min
@Temperature 100 °C
1.50 - 2.00 hour
@Temperature 212 °F
Optimum, followed by a post cure of 2-3 hours at 100-125°C
Shelf Life 3.00 - 6.00 Month
@Temperature 4.00 - 10.0 °C
3.00 - 6.00 Month
@Temperature 39.2 - 50.0 °F
in a refrigerator
 
Descriptive Properties
Thixotropic index5.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5907 / 306796

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.