MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX910 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 910 resin is non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). NORYL GTX910 resin exhibits excellent chemical resistance and is an excellent candidate for automotive applications such as plastic/metal hybrid components, rail extensions, crash cans, wheel covers, and energy absorbers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Aesthetics & Visual effects,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Density 1.107 g/ccASTM D792
Moisture Absorption 0.0700 %Injection Molding
 0.500 %23°C/50% RH/24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.0 %23°C/50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cmannealed 130C 1hr; ASTM D955
 0.011 - 0.013 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength at Break 55.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 59.0 MPa50 mm/min; ASTM D638
Elongation at Break 60 %50 mm/min; ASTM D638
Flexural Strength 95.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2240 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 240 JASTM D256
 133 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 50.0 Jpeak; ASTM D3763
 39.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 400 - 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 126 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 126 µm/m-°C
@Temperature 60.0 - 138 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 232 °CRate B/50; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 305 °C
Zone 2 270 - 305 °C
Zone 3 275 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82159 / 290106

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.