MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Primex Plastics Prime Tuff-X STF Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Prime Tuff-X STF consists of a Thermoplastic elastomer skin laminated to closed-cell, cross-linked polyolefin foam that is then laminated to our Tuff-X rigid substrate. Low gloss and soft feel eliminate the need for soft-touch paint. (<5% after forming) It also helps eliminate the squeak and rattle that is characteristic of Styrenics. Recycling of unpainted scrap is possible with no loss of properties.

Applications: Tuff-X STF is ideal for interior and exterior components, including center consoles, instrument panels, door panels, and many others. This addresses the customers’ desire for a low-gloss, soft feel material to soften interior and exterior applications in markets such as agricultural equipment, marine, heavy trucks, RV cabs, and others, while utilizing a thermoplastic, recyclable material.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0264 g/cc0.0264 g/ccISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.4 MPa3100 psisub; ISO 527-2
Flexural Modulus 2.07 GPa300 ksisub; ISO 178
Instrumented Impact Total Energy  51.9 J
@Temperature 23.0 °C
38.3 ft-lb
@Temperature 73.4 °F
ASTM D3763
 63.0 J
@Temperature -15.0 °C
46.5 ft-lb
@Temperature 5.00 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.5 µm/m-°C27.5 µin/in-°F
Deflection Temperature at 0.46 MPa (66 psi) 116 °C240 °FSubstrate; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FSubstrate; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM035 / 278506

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.