MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Eastman Eastar MN021 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: Eastar™ Copolyester MN021 Natural has been tested for FDA/ISO 10993 and USP Class VI Biological Evaluation testing after Gamma and EtO sterilization. Eastar™ copolyester MN021 Natural is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has a relatively high flex modulus and yield strength. This product does not contain a mold release. It is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystallized. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED

Applications/Uses:

  • Drug Delivery
  • Labware
  • Medical
Key Attributes:
  • Chemical resistance to most medical solvents including lipids and IPA
  • Gamma and E-beam color stability

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength at Break 25.0 MPaASTM D638
Tensile Strength, Yield 58.0 MPaASTM D638
Elongation at Break 120 %ASTM D638
Tensile Modulus 2.40 GPaASTM D638
Flexural Yield Strength 84.0 MPaASTM D790
Flexural Modulus 2.50 GPaASTM D790
Izod Impact, Notched 0.270 J/cm
@Temperature -40.0 °C
ASTM D256
 40.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 1.60 J
@Thickness 2.50 mm,
Temperature -40.0 °C
max load; ASTM D3763
 2.10 J
@Thickness 3.20 mm,
Temperature -40.0 °C
max load; ASTM D3763
 26.0 J
@Thickness 2.50 mm,
Temperature 23.0 °C
max load; ASTM D3763
 31.0 J
@Thickness 3.20 mm,
Temperature 23.0 °C
max load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Transmission, Visible 84 %Total Transmittance; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 275 - 295 °C
Mold Temperature 10.0 - 30.0 °C
Drying Temperature 150 - 160 °C
Dry Time 4 - 6 hour
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman DuraStar DS1000 Polymer, Natural
Eastman Eastar DN003 PCTG Copolyester
Eastman DuraStar DS1900HF Polymer, Natural
Eastman Eastalloy DA003 PC+PCTG Copolyester/Polycarbonate
Eastman Eastar DN004 PCTG Copolyester

PE9051 / 35107

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.