High flow Polyetherimide (Tg 217°C) with low level of transparent mold release. Very low outgassing and plateout for optimally reduced need for mold cleaning. May be beneficial for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 204°C (SABIC IP method). Features: Low Creep Sensitivity,High Heat Resistance,Good dimensional stability,Good Mold Release,Aesthetics & Visual effects Information provided by SABIC |