MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

PolyLabs U-212 Flexible Polyurethane (PU) Foam
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Flexible Polyurethane Foam is a versatile compound, designed for various applications. It is utilized in applications that require a soft, medium-tear flexible foam. It is especially useful in products where hardness can easily be varied. Common products include toy balls, wrist rests, and padding applications such as seat cushions.

Information provided by PolyLabs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.150 - 0.250 g/cc0.00542 - 0.00903 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 30 - 4530 - 45
Tensile Strength 0.414 - 0.448 MPa60.0 - 65.0 psi
Elongation at Break 110 - 130 %110 - 130 %
Tear Strength 0.877 - 1.23 kN/m5.00 - 7.00 pliDie C
Compression Set <= 10 %<= 10 %
 
Descriptive Properties
Oil Resistancy>250,000
Oil Swell<15%ASTM #3
 13%Fuel F, Diesel
 37%Fuel B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYLA965 / 265889

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.