MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ LUBRICOMP™ Compound LFL36E Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP LUBRICOMP LFL36E compound is based on Polyetheretherketone (PEEK) resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant, Easy Molding.

Features: Wear resistant,Good Moldability,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ASTM D792
Moisture Absorption 0.100 %0.100 %Injection Molding
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psi5 mm/min; ASTM D638
 177 MPa25700 psi5 mm/min; ISO 527
Tensile Strength, Yield 176 MPa25500 psi5 mm/min; ASTM D638
Elongation at Break 2.0 %2.0 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ASTM D638
Tensile Modulus 12.24 GPa1775 ksi1 mm/min; ISO 527
Flexural Strength 263 MPa38100 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 11.36 GPa1648 ksi2 mm/min; ISO 178
 11.7 GPa1700 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 103 J76.0 ft-lbASTM D256
Izod Impact, Unnotched 8.61 J/cm16.1 ft-lb/inASTM D4812
Dart Drop, Total Energy 13.0 J9.59 ft-lbASTM D3763
Coefficient of Friction, Dynamic 0.490.49ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.730.73ASTM D3702 Modified: Manual
K (wear) Factor 18.1 x 10-8 mm³/N-M9.00 x 10-10 in³-min/ft-lb-hrRing; ASTM D3702 Modified: Manual
 129 x 10-8 mm³/N-M64.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
10.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow 36.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
20.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 337 °C639 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 339 °C
@Thickness 3.20 mm
642 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 322 °C612 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 327 °C
@Thickness 3.20 mm
621 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 365 - 375 °C689 - 707 °F
Zone 3 380 - 395 °C716 - 743 °F
Melt Temperature 380 - 390 °C716 - 734 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 60 - 100 rpm60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80878 / 288825

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.