MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huber Martoxid® MDLS-6 Calcined Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Martoxid® MDLS-6 calcined aluminum oxide is a ground aluminum oxide with high Al2O3-content for chemical and mechanical resistant components. Filler in epoxy resin high voltage insulator parts (GIS) with excellent electrical and mechanical properties.

CAS No.: 1344-28-1

EC/EINECS No.: 215-691-6

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density <= 0.800 g/cc<= 0.0289 lb/in³
Particle Size 0.50 - 2.5 µm0.50 - 2.5 µmd10, Cilas 1064
 3.0 - 4.0 µm3.0 - 4.0 µmd50, Cilas 1064
 7.0 - 14 µm7.0 - 14 µmd90, Cilas 1064
 >= 45 µm>= 45 µm<1 percent
Specific Surface Area 0.50 - 1.4 m²/g0.50 - 1.4 m²/gBET
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 10000 ohm-cm>= 10000 ohm-cm25 % in H2O
 
Component Elements PropertiesMetricEnglishComments
Al2O3 >= 95 %>= 95 %a-Al2O3
CaO 0.030 %0.030 %
Fe2O3 0.030 %0.030 %
Loss on Ignition(%) <= 0.10 %<= 0.10 %
Na2O <= 0.020 %<= 0.020 %soluble
 0.030 %0.030 %total
SiO2 0.060 %0.060 %
 
Descriptive Properties
Al(OH)3 (%)99.8
FunctionalityElectrical Resistance
 Inert filler
 Thermal Conductivity
Market/Application: E & E, InfrastructureSemiconductors / Insulators
Market/Application: ThermosetsEpoxy
Primary Crystal4 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER808 / 300914

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.