MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ FR LUX9610 PC (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN LUX9610 is an injection moldable polycarbonate (PC) with an MVR (300°C/1.2kg) 7. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0@1.5mm rating. This is a UV stabilized, transparent grade with high optical clarity and impact resistance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.07 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cmSABIC method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 65.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa50 mm/min; ASTM D638
Elongation at Break 110 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2320 MPa50 mm/min; ASTM D638
Flexural Yield Strength 95.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 760 J/mASTM D256
 123 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D4812
Dart Drop, Total Energy 75.0 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI 60 - 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/120; ISO 306
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 115 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °CInjection Molding
Zone 1 260 - 280 °C
Zone 2 270 - 295 °C
Zone 3 280 - 305 °C
Melt Temperature 280 - 305 °C
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10645 / 244112

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.