MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC SABIC® PS 325 PS (Global)
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: PS 325 is High Impact Polystyrene manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resistance property. It is generally opaque in color. It is having medium flow characteristics with high tensile and flexural strength with medium heat deflection and vicat temperatures.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³ASTM D1895
Density 1.04 g/cc
@Temperature 23.0 °C
0.0376 lb/in³
@Temperature 73.4 °F
Load Density; ASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 6060Based on Injection molded specimens.; ASTM D785
Hardness, Rockwell M 1010Based on Injection molded specimens.; ASTM D785
Tensile Strength, Yield 22.0 MPa3190 psiBased on Injection molded specimens.; ASTM D638
Elongation at Yield 50 %50 %Based on Injection molded specimens.; ASTM D638
Tensile Modulus 2.157 GPa312.8 ksiBased on Injection molded specimens.; ASTM D638
Flexural Strength 35.0 MPa5080 psiBased on Injection molded specimens.; ASTM D790
Flexural Modulus 2.353 GPa341.3 ksiASTM D790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inBased on Injection molded specimens.; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C199 °FAnnealed; ASTM D648
Vicat Softening Point 95.0 °C203 °FRate A/50°C; ASTM D1525
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11602 / 245069

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.