OKULEN® 2000 – H – FN9252 is premier UHMW-PE Polymer containing a unique antioxidant which protects the material from breaking apart at extreme temperatures. This material grade is used in high temp applications were normal UHMW-PE fails. The material grade is used in high temp applications were normal UHMW-PE fails. The enhanced material was designed to still operate effectively under lower load, with a temperature range peaking 150°C for a short time. Properties: Long term operating temperature possible at Peak range 150°C (only at lower loads); EU 1935/2004 & 10/2011 – conform; FDA – conform; up to 10 x longer life time at higher temperatures than any standard grade of UHMW-PE Color: white FN9252 Range of applications: Bakeries (bun racks); Food industry; For windows (with arches) Information provided by Okulen |