System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Copper, UNS C27200 (Yellow Brass 63.5%), OS025
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Brass
Material Notes:
Nominal grain size = 0.025 mm.
Applications:
typical brass applications such as fasteners, cold headed parts, pump cylinder liners, and heat exchanger shells. Registered with US EPA as antimicrobial.
Key Words:
CDA 272
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.44
g/cc
Thickness
65.0
microns
tube section size, as-tested
Mechanical Properties
Original Value
Comments
Hardness, Rockwell F
82
Tensile Strength
56.0
ksi
Tensile Strength, Yield
23.0
ksi
@Strain 0.5 %
Elongation at Break
50 %
Modulus of Elasticity
15000
ksi
Poissons Ratio
0.34
Calculated
Shear Modulus
5600
ksi
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.00000620
ohm-cm
@Temperature 20.0 °C
27.6% IACS
Thermal Properties
Original Value
Comments
CTE, linear
11.4
µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity
0.0900
BTU/lb-°F
@Temperature 20.0 °C
Thermal Conductivity
804
BTU-in/hr-ft²-°F
@Temperature 20.0 °C
Melting Point
<=
1680
°F
Liquidus
Liquidus
1680
°F
Component Elements Properties
Original Value
Comments
Copper, Cu
62 - 65 %
Iron, Fe
<= 0.070 %
Lead, Pb
<= 0.070 %
Other, total
<= 0.30 %
Zinc, Zn
34.6 - 38 %
as remainder
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
MC27200b2 / 291097
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.