MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin 731 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ 731 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits good surface appearance, high ductility, and good impact resistance along with low moisture absorption, creep resistance, dimensional stability, and hydrolytic stability. NORYL 731 resin is an excellent candidate for a variety of applications.

Features: Hydrolytic Stability,Low Creep Sensitivity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
Moisture Absorption 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %ISO 62-1
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 100 MPaH358/30; ISO 2039-1
Tensile Strength at Break 50.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
Elongation at Break 30 %50 mm/min; ISO 527
Elongation at Yield 5.0 %50 mm/min; ISO 527
Tensile Modulus 2300 MPa1 mm/min; ISO 527
Flexural Strength 75.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 65CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.6
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 19.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 1e+6 Hz
IEC 60250
 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 VIEC 60112
 250 - 400 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
 30 - 60 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.220 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
 133 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 130 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 115 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 135 °CRate B/50; ISO 306
 140 °CRate B/120; ISO 306
 145 °CRate A/50; ISO 306
UL RTI, Electrical 105 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 105 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Oxygen Index 22 %ISO 4589
Glow Wire Flammability Index 750 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CCalibrator Temperature
Nozzle Temperature 260 - 280 °C
Zone 1 220 - 240 °CProfile Extrusion
Zone 2 230 - 250 °CProfile Extrusion
 260 - 280 °C
Zone 3 250 - 270 °CProfile Extrusion
 280 - 300 °C
Zone 4 250 - 270 °CProfile Extrusion
Adapter Temperature 250 - 270 °CProfile Extrusion
Die Temperature 250 - 270 °CProfile Extrusion
Melt Temperature 250 - 270 °CProfile Extrusion
 280 - 300 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 110 °CProfile Extrusion
 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
 2.00 - 3.00 hourProfile Extrusion
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature
 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82243 / 290190

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.