LNP LUBRICOMP JZL012 compound is based on Polyethersulfone (PES) resin containing proprietary filler, PTFE. Added features of this grade include: Internally Lubricated, Wear Resistant, Dimensional Control. Features: Internally Lubricated,Good dimensional stability,Wear resistant Information provided by SABIC |