MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR CY6110 PC+ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CY6110 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an impact modified, high flow injection moldable, non chlorinated/brominated flame retardant grade. It features good hydrostability and has a UL94 V0@1.5mm and 5VB@2.5mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Water Absorption 0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPa50 mm/min; ISO 527
 47.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa50 mm/min; ISO 527
 63.0 MPa50 mm/min; ASTM D638
Elongation at Break 35 %50 mm/min; ISO 527
 65 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ISO 527
 4.1 %50 mm/min; ASTM D638
Tensile Modulus 2750 MPa1mm/min; ISO 527
 2760 MPa5 mm/min; ASTM D638
Flexural Yield Strength 94.0 MPa2 mm/min; ISO 178
Flexural Modulus 2440 MPa2 mm/min; ISO 178
Izod Impact, Notched 475 J/mASTM D256
 100 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 33.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
 2.9
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 31.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 46.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0070
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 8.00 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 8.00 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 104 °CRate B/50; ISO 306
 106 °CRate B/120; ISO 306
UL RTI, Electrical 85.0 °CUL 746B
UL RTI, Mechanical with Impact 85.0 °CUL 746B
UL RTI, Mechanical without Impact 85.0 °CUL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
UL 94 by SABIC-IP
 V-0
@Thickness 1.50 mm
UL 94
 5VB
@Thickness 2.50 mm
UL 94
Oxygen Index 31 %ISO 4589
Glow Wire Test 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
IEC 60695-2-13
 775 °C
@Thickness 0.750 mm
IEC 60695-2-13
 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CHopper Temperature
Nozzle Temperature 250 - 300 °CInjection Molding
Zone 1 230 - 280 °C
Zone 2 240 - 290 °C
Zone 3 250 - 300 °C
Melt Temperature 250 - 300 °C
Mold Temperature 60.0 - 85.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %
Vent Depth 0.00300 - 0.00750 cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10798 / 244265

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.