MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F584™ Modified Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Wet is 30 days of humidity conditioning at 160°F (71°C) and 95% relative humidity.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.219 g/cc0.04404 lb/in³
Viscosity  30000 cP
@Temperature 140 °C,
Time 4500 sec
30000 cP
@Temperature 284 °F,
Time 1.25 hour
Rheometrics Curve of F584 4°F/Min (2°C/Min), 10 Rad/Sec, RDS-7700, 50 mm Plates
 100000 cP
@Temperature 170 °C,
Time 4790 sec
100000 cP
@Temperature 338 °F,
Time 1.33 hour
Rheometrics Curve of F584 4°F/Min (2°C/Min), 10 Rad/Sec, RDS-7700, 50 mm Plates
 9.00e+7 cP
@Temperature 25.0 °C,
Time 0.000 sec
9.00e+7 cP
@Temperature 77.0 °F,
Time 0.000 hour
Rheometrics Curve of F584 4°F/Min (2°C/Min), 10 Rad/Sec, RDS-7700, 50 mm Plates
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 73.1 MPa10600 psi
Elongation at Break 1.80 %1.80 %
Tensile Modulus 4.14 GPa600 ksi
Poissons Ratio 0.3500.350
Fracture Toughness 0.901 MPa-m½0.820 ksi-in½K1C
Tensile Impact Strength 2.10 kJ/m²1.00 ft-lb/in²Strain energy release rate, G1C
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 121 °C250 °Fwet (RDS)
 171 °C340 °Fdry (RDS)
 
Processing PropertiesMetricEnglishComments
Gel Time  2.00 - 8.00 min
@Temperature 177 °C
2.00 - 8.00 min
@Temperature 351 °F
 19.0 - 25.0 min
@Temperature 149 °C
19.0 - 25.0 min
@Temperature 300 °F
Shelf Life  3.00 Month
@Temperature 4.00 °C
3.00 Month
@Temperature 39.2 °F
 6.00 Month
@Temperature -18.0 °C
6.00 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9124 / 322280

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.