System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Toyobo Celstran® PA6-GF40-01 AF3001 Natural Nylon 6, 40% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 40% Glass Fiber Filled
Material Notes:
Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America
Filler/Reinforcement: Glass Fiber
Forms: Pellets
Processing Method: Injection Molding
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.45
g/cc
0.0524
lb/in³
ISO 1183
Maximum Moisture Content
0.18
0.18
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
230
MPa
33400
psi
ISO 527-2/5
Elongation at Break
2.4 %
2.4 %
ISO 527-2/5
Tensile Modulus
13.0
GPa
1890
ksi
ISO 527-1
Flexural Strength
370
MPa
53700
psi
ISO 178
Flexural Modulus
11.3
GPa
1640
ksi
ISO 178
Izod Impact, Notched (ISO)
35.7
kJ/m²
17.0
ft-lb/in²
ISO 180/1A
Processing Properties
Metric
English
Comments
Processing Temperature
70.0
-
80.0
°C
158
-
176
°F
Hopper
Feed Temperature
20.0
-
50.0
°C
68.0
-
122
°F
Injection
Rear Barrel Temperature
265
-
275
°C
509
-
527
°F
Middle Barrel Temperature
270
-
275
°C
518
-
527
°F
Front Barrel Temperature
275
-
280
°C
527
-
536
°F
Nozzle Temperature
275
-
280
°C
527
-
536
°F
Zone 4
275
-
280
°C
527
-
536
°F
Injection
Melt Temperature
270
-
280
°C
518
-
536
°F
Mold Temperature
80.0
-
100
°C
176
-
212
°F
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PHCQ6227 / 310920
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.