LNP* THERMOCOMP* D351RC compound is based on Polycarbonate resin containing Glass Fiber and Flame Retardant. Added features of this material includes high modulus, good flatness, good impact performance, Non-Halogenated Flame Retardant, PCR content up to 35%.Information provided by SABIC |