FLEX NORYL™ WCP841 resin is flexible, non-reinforced injection moldable blend of polyphenylene ether (PPE) + thermoplastic elastomer (TPE). This material contains non-halogenated flame retardant and carries a UL94 flame rating of V0 at 6mm. FLEX NORYL WCP841 resin is intended for evaluation in over-molding applications such as plugs, strain reliefs, and connectors. It has a Shore A Hardness reading of 84 and exhibits low specific gravity, very low water absorption, and dimensional stability. Features: Flexible,Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Good Processability,Ductile Information provided by SABIC |