MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Lustran® 256/Lustran® 752 Blended ABS Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS

Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 34.0 MPaASTM-D638
Tensile Modulus 2.00 GPaASTM-D638
Flexural Yield Strength 61.0 MPaASTM-D790
Flexural Modulus 2000 MPaASTM-D790
Izod Impact, Notched 91.0 J/m
@Thickness 3.20 mm,
Temperature -40.0 °C
ASTM-D256
 160 J/m
@Thickness 3.20 mm,
Temperature -18.0 °C
ASTM-D256
 299 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM-D256
Instrumented Impact Total Energy 19.0 J
@Temperature -40.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 26.0 J
@Temperature -18.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 43.0 J
@Temperature 23.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
Instrumented Impact Energy at Peak 18.0 J
@Temperature -40.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 23.0 J
@Temperature -18.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 31.0 J
@Temperature 23.0 °C
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); ASTM-D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °CUnannealed; ASTM-D648
 
Optical PropertiesOriginal ValueComments
Gloss 40 %Formed, Angle 60°; ASTM-D523
 85 %Sheet, Angle 60°; ASTM-D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond Centrex® 814 General Purpose Injection Molding Grade
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Lotte Advanced Materials Starex® SR-7300 ABS/PET, Unreinforced
Polyram RamLloy PJ701 ABS/ASA, General Purpose
Polyram RamShine PV701 ABS, UV Stabilized

PINEA956 / 107227

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.